bandersen: 30A16: 10BP4 CRT
bandersen: 30A16:
bandersen: 30A16:
bandersen: 30A16: HV cage
bandersen: 30A16: Cadmium plating ?
bandersen: 30A16:
bandersen: 30A16:
bandersen: 30A16: veneer damage
bandersen: 30A16: veneer damage
bandersen: 30A16: foam gasket
bandersen: admiral 30A16
bandersen: 30A16: Upgrade ad
bandersen: 30A16: Lower chassis and speaker
bandersen: 30A16: bottom
bandersen: 30A16: Decals in good shape
bandersen: 30A16: Channel lineup
bandersen: 30A16: So nice to have all the knobs
bandersen: 30A16: Front/side view
bandersen: 30A16: Oxidized cadmium plating
bandersen: 30A16: Wiping on rust-remover
bandersen: 30A16: Oxidation comes right off
bandersen: 30A16: Neutralizing acid
bandersen: 30A16: It's a stinky process
bandersen: 30A16: Polishing the cadmium
bandersen: 30A16: Nice and shiny
bandersen: 30A16: Pouring solution onto a paper towel
bandersen: 30A16: Top chassis
bandersen: 30A16: Decal reference
bandersen: 30A16: Label
bandersen: Unrestored Admiral 30A1 chassis